Polymer Property : Nozzle Temperature = 241 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 210 - 241 °C
410 - 465 °F
ExxonMobil Santoprene® 243-50 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
Nozzle Temperature 210 - 241 °C
410 - 465 °F
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Nozzle Temperature 210 - 241 °C
410 - 465 °F
ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Nozzle Temperature 210 - 241 °C
410 - 465 °F
ExxonMobil Santoprene® 203-50 Thermoplastic Elastomer
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Nozzle Temperature 210 - 241 °C
410 - 465 °F
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer  (discontinued **)
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..