Polymer Property : Nozzle Temperature = 246 °C
Polymer Property :
Nozzle Temperature =
246 °C
Product List
Processing Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties
Metric
English
Comments
Nozzle Temperature
218
-
246
°C
425
-
475
°F
Clariant ABS4500 ABS, High Impact
Data provided by Clariant Masterbatches