Polymer Property : Nozzle Temperature = 268 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 268 - 282 °C
515 - 540 °F
Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced
Notes: 25% Mineral - 15% Glass; Excellent stiffness and strength, especially at high temperatures, with improved warpage control over glass reinforced products; FMVSS Flammability: Passes, FMVSS 302..
Nozzle Temperature 268 - 279 °C
515 - 535 °F
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated
Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex
Nozzle Temperature 268 - 282 °C
515 - 540 °F
Teknor Apex Chemlon® 133 G Nylon 66, 33% Short Glass Fiber Filled
Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex