Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 177 - 199 °C | 350 - 390 °F | |
Elastocon TPE Technologies Elastocon® 8038N Thermoplastic Elastomer Elastocon® 8038N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8038N is FDA compliant and well suited.. |