Nozzle Temperature 223 °C
433 °F
Injection
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol