Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 229 °C | 444 °F | Injection |
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Nozzle Temperature | 229 °C | 444 °F | Injection |
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol. |