Processing Properties Metric English Comments
Nozzle Temperature 420 - 450 °C
788 - 842 °F
Kraton® G7705 GI-B (SEBS) Compound
Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Nozzle Temperature 420 - 450 °C
788 - 842 °F
Kraton® G7705 GI-N (SEBS) Compound
Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Nozzle Temperature 420 - 450 °C
788 - 842 °F
Kraton® G7820 GU-N (SEBS) Compound
Description: Kraton G7820 GU-N is an easy processing, general purpose 90 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Nozzle Temperature 420 - 450 °C
788 - 842 °F
Kraton® G7720 GI-N (SEBS) Compound
Description: Kraton G7720 GI-N is an easy processing, general purpose 57 Shore a hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..