Processing Properties Metric English Comments
Nozzle Temperature 305 °C
581 °F
Typical Die Temp.
DuPont Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
4 wt% Methacrylic Acid.Nucrel® 0411HS (High-Speed) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating..
Nozzle Temperature 305 °C
581 °F
Typical Die Temp.
DuPont Nucrel® 910 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
8.7 wt% Methacrylic Acid.Nucrel® 0910 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment de..
Nozzle Temperature 305 °C
581 °F
Typical Die Temp.
DuPont Nucrel® 407 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
4 wt% Methacrylic Acid.Nucrel® 0407 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment desi..
Nozzle Temperature 305 °C
581 °F
Typical Die Temp.
DuPont Nucrel® 0609HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating  (discontinue
6 wt% Methacrylic Acid.Nucrel® 0609HS* (High-Speed) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminatin..