Processing Properties Metric English Comments
Nozzle Temperature 304 - 332 °C
580 - 630 °F
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 304 - 332 °C
580 - 630 °F
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 304 - 332 °C
580 - 630 °F
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 304 - 332 °C
580 - 630 °F
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 254 - 332 °C
490 - 630 °F
Average value: 284 °C Grade Count:18
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
Nozzle Temperature 310 - 332 °C
590 - 630 °F
LTL Color Compounds ColorFast® PCGF120 Polycarbonate, 20% Glass-Filled
20% glass-filled grade, good balance of impact and mechanical propertiesAll information provided by LTL Color Compounders, Inc.
Nozzle Temperature 310 - 332 °C
590 - 630 °F
LTL Color Compounds ColorFast® PCGF130 Polycarbonate, 30% Glass-Filled
30% glass-filled grade polycarbonateAll information provided by LTL Color Compounders, Inc.
Nozzle Temperature 304 - 332 °C
580 - 630 °F
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 304 - 332 °C
580 - 630 °F
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 304 - 332 °C
580 - 630 °F
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 304 - 332 °C
580 - 630 °F
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).