Processing Properties Metric English Comments
Mold Temperature 83.0 °C
181 °F
Ejection temperature
Styrolution Terluran® GP-35 ABS
Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an..