Processing Properties Metric English Comments
Mold Temperature 193 - 207 °C
379 - 405 °F
Blow Molding
PolyOne Geon™ Vinyl Packaging PK8 WHITE 1081 Polyvinyl Chloride, Rigid (PVC, Rigid)
The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne
Mold Temperature 193 - 210 °C
379 - 410 °F
Blow Molding
PolyOne Geon™ Vinyl Packaging VB7 White 215 Polyvinyl Chloride, Rigid (PVC, Rigid)
A rigid PVC Compound designed for extrusion blow molding balusters for railings.Information provided by PolyOne
Mold Temperature 193 - 210 °C
379 - 410 °F
Blow Molding
PolyOne Geon™ Vinyl Packaging VEO-184 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne