Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 51.7 - 57.2 °C | 125 - 135 °F | |
LTL Color Compounds Surlyn Reflection Series® SURSG201UG Surlyn Resin/Nylon 6 Alloy A patented alloy of DuPont™ Surlyn® resin and nylon 6 for applications that require a high gloss, molded in color surface finish directly from the mold.All information provided by LTL Color .. |
|||
Mold Temperature | 37.8 - 57.2 °C | 100 - 135 °F | |
ACC EP IS EPI Engineered Polymers Integral Skin Flexible Foam EP-IS is integral skin flexible foam, “Powered by Reactamine ® Technology”, designed to give excellent surface skin. EP-IS contains cyclopentane as its blowing agent, which conforms to EPA standa.. |