Polymer Property : Rear Barrel Temperature = 215 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 215 °C
419 °F
NYCOA 1637 PA 6
plasticized and heat stabilized extrusion grade for the wire jacketing industry to 7,000+ fpm. UL Flammability Component listing for use as cable jacketing.Information provided by NYCOA, Inc.
Rear Barrel Temperature 215 °C
419 °F
NYCOA 2001 PA 6
high melt strength general extrusion and molding grade of nylon 6Information provided by NYCOA, Inc.
Rear Barrel Temperature 215 °C
419 °F
NYCOA 2038 10% Glass Filled Nylon 6
10% glass filled very high viscosity nylon 6Information provided by NYCOA, Inc.
Rear Barrel Temperature 215 - 235 °C
419 - 455 °F
Injection Molding
LG Chemical KEYFLEX BT 1068D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Rear Barrel Temperature 215 - 235 °C
419 - 455 °F
Injection Molding
LG Chemical KEYFLEX BT 3047D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Rear Barrel Temperature 215 - 250 °C
419 - 482 °F
Injection Molding
LG Chemical LUMID GP1300AP PA6, Plasticized
Feature: Injection Molding, PA6, PlasticizedApplication: Automotive PartsInformation provided by LG Chemical
Rear Barrel Temperature 215 - 240 °C
419 - 464 °F
Extrusion
Ineos ABS Lustran® LK197 ABS, Extrusion Grade
Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e..