Polymer Property : Rear Barrel Temperature = 279 °C
Polymer Property :
Rear Barrel Temperature =
279 °C
Product List
Processing Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
257
-
279
°C
495
-
535
°F
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).