Polymer Property : Rear Barrel Temperature = 382 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 360 - 382 °C
680 - 720 °F
LNP ULTEM® SMU5806 Polyetherimide, 8% Carbon Fiber Reinforcement  (discontinued **)
Features: Low ShrinkageForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still..