Processing Properties Metric English Comments
Rear Barrel Temperature 196 - 204 °C
385 - 399 °F
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE)
Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat ..