Polymer Property : Rear Barrel Temperature = 425 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 188 - 218 °C
370 - 425 °F
Star Plastics ABS3030 Molding Grade ABS
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 188 - 218 °C
370 - 425 °F
Star Plastics ABS405 Extrusion Grade ABS
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 188 - 218 °C
370 - 425 °F
Star Plastics ABS5035 Molding Grade ABS
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 188 - 218 °C
370 - 425 °F
Star Plastics ABS9020 Molding Grade ABS
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 188 - 218 °C
370 - 425 °F
Star Plastics ABSGF10 Molding Grade ABS With 10% Glass
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 188 - 218 °C
370 - 425 °F
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 188 - 218 °C
370 - 425 °F
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 188 - 218 °C
370 - 425 °F
Star Plastics ABSHFL Molding Grade ABS High Flow
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 188 - 218 °C
370 - 425 °F
Star Plastics ABSLG3030 Molding Grade ABS, Low Gloss
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 188 - 218 °C
370 - 425 °F
Star Plastics ABSLG5035 Molding Grade ABS, Low Gloss
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 188 - 218 °C
370 - 425 °F
Star Plastics ABS3545 Molding Grade ABS
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 188 - 218 °C
370 - 425 °F
Star Plastics ABS448T Molding Grade ABS
Information provided by Star Plastics, Inc.