Polymer Property : Drying Temperature = 82.2 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 82.2 °C
180 °F
PolyOne Nymax™ GF 1800 43 Black 22 Polyamide 612 (Nylon 612)
Property data for molded test bars: Dry as MoldedInformation provided by PolyOne
Drying Temperature 82.2 °C
180 °F
PolyOne Nymax™ GMF 604 40 UV Black 115 1 X 1 Polyamide 6 (Nylon 6)
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor..
Drying Temperature 82.2 °C
180 °F
ExxonMobil Santoprene® 221-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Drying Temperature 82.2 °C
180 °F
ExxonMobil Santoprene® 261-87 Thermoplastic Elastomer  (discontinued **)
A hard, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance for use in wet electrical wire and cable applications. This gra..
Drying Temperature 82.2 °C
180 °F
ExxonMobil Vyram™ 9103-45 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Drying Temperature 82.2 °C
180 °F
PolyOne Nymax™ GF 1200 60 HS Black 22 Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Drying Temperature 82.2 °C
180 °F
PolyOne Nymax™ GF 1200 A 33 Natural Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Drying Temperature 82.2 °C
180 °F
Average value: 82.2 °C Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Drying Temperature 82.2 °C
180 °F
PolyOne Edgetek® AT-10GB/000 Black Acetal-Copolymer, Glass Bead Filled  (discontinued **)
Description/Features:Glass Bead FilledInformation provided by PolyOne Corporation.
Drying Temperature 82.2 °C
180 °F
LTL Color Compounds ColorFast® ACR100 Polymethylmethacrylate
High heat injection molding grade of PMMAAll information provided by LTL Color Compounders, Inc.
Drying Temperature 82.2 - 93.3 °C
180 - 200 °F
During prolong interruptions the hopper dryer temperature should be reduced to 65ºC or lower.
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
Drying Temperature 82.2 - 85.0 °C
180 - 185 °F
Styron MAGNUMâ„¢ 357 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi..
Drying Temperature 82.2 °C
180 °F
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap..
Drying Temperature 82.2 °C
180 °F
ExxonMobil Santoprene® 121-50M100 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult ..
Drying Temperature 82.2 °C
180 °F
ExxonMobil Santoprene® 251-80W232 Thermoplastic Elastomer
A soft, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard..
Drying Temperature 82.2 - 92.2 °C
180 - 198 °F
Diamond Polymers ASA M-143
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Drying Temperature 82.2 °C
180 °F
Styron Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS)
Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance to processability, impact resistance and heat resistance as imparted by the various polymer compositions...
Drying Temperature 82.2 °C
180 °F
PolyOne Edgetek® UR-20GF/000 Thermoplastic Elastomer - TPU, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.