Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 102 °C | 216 °F | |
Eastman Eastar Copolyester K3000 PETG Copolyester
(discontinued **) EASTAR K3000 Copolyester is a cost effective, high-performance, water-clear material that provides the necessary performance for the appliance standards. Other desirable characteristics are good ch.. |