Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 45.0 °C

@Time 14400 sec
113 °F

@Time 4.00 hour
NatureWorks® Ingeo™ 4060D Sealant Grade PLA
PLA (polylactide) polymer 4060D can be coextruded with other PLA resin to form a sealant layer for biaxially oriented PLA film. This resin has excellent heat seal and hot tack performance with a sea..