Polymer Property : Drying Temperature = 49.0 °C
Polymer Property :
Drying Temperature =
49.0 °C
Product List
Processing Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties
Metric
English
Comments
Drying Temperature
49.0
-
66.0
°C
120
-
151
°F
PolyOne Lubri-Tech™ SY-000/05T High Impact Styrene - 5% PTFE (discontinued **)