Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 99.0 - 110 °C | 210 - 230 °F | air dew point <-40°C |
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Drying Temperature | 99.0 - 110 °C | 210 - 230 °F | air dew point <-40°C |
Lubrizol Pellethane® 2363-75D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Drying Temperature | 99.0 - 110 °C | 210 - 230 °F | air dew point <-40°C |
Lubrizol Estane® 2102-65D Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Drying Temperature | 99.0 - 110 °C | 210 - 230 °F | air dew point <-40°C |
Lubrizol Estane® 2103-65D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low temperature impactAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |