Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 7 - 10 hour | 7 - 10 hour | Hydraulic Set Time, Final |
Zircar Ceramics ZIRALCAST 95 Alumina Refractory Castable Hydraulically setting castable refractory containing high purity fused alumina "bubbles". This low density castable can be used like concrete and produces ceramic bodies useful in a range of applica.. |
|||
Dry Time | 8 - 10 hour | 8 - 10 hour | Demold time, catalyzed with Moldmaster Purple |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Dry Time | 8 - 10 hour | 8 - 10 hour | Demold time, catalyzed with Moldmaster Purple |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |