Polymer Property : Back Pressure = 0.600 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 0.600 - 1.20 MPa
87.0 - 174 psi
Injection
Alliance Polymers Zythane™ 4045D Thermoplastic Polyurethane Elastomer
Zythane™ 4045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Back Pressure 0.600 - 1.40 MPa
87.0 - 203 psi
Injection
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer
Zythane™ 4060D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Back Pressure 0.600 - 1.40 MPa
87.0 - 203 psi
Injection
Alliance Polymers Zythane™ 4065D Thermoplastic Polyurethane Elastomer
Zythane™ 4065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Back Pressure 0.600 - 1.20 MPa
87.0 - 174 psi
Injection
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer
Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Back Pressure 0.600 - 1.20 MPa
87.0 - 174 psi
Injection
Alliance Polymers Zythane™ 6045D Thermoplastic Polyurethane Elastomer
Zythane™ 6045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Back Pressure 0.600 - 1.40 MPa
87.0 - 203 psi
Injection
Alliance Polymers Zythane™ 6055D Thermoplastic Polyurethane Elastomer
Zythane™ 6055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Back Pressure 0.600 - 1.40 MPa
87.0 - 203 psi
Injection
Alliance Polymers Zythane™ 6065D Thermoplastic Polyurethane Elastomer
Zythane™ 6065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Back Pressure 0.600 - 1.20 MPa
87.0 - 174 psi
Injection
Alliance Polymers Zythane™ 7045A Thermoplastic Polyurethane Elastomer
Zythane™ 7045A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Back Pressure 0.600 - 1.40 MPa
87.0 - 203 psi
Injection
Alliance Polymers Zythane™ 7055D Thermoplastic Polyurethane Elastomer
Zythane™ 7055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Back Pressure 0.600 - 1.40 MPa
87.0 - 203 psi
Injection
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer
Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..