Processing Properties Metric English Comments
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ P75A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P75A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ P75A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P75A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ P80A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ P80A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ P70A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P70A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..