Polymer Property : Back Pressure = 10200 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 50.0 - 70.0 MPa
7250 - 10200 psi
Molding Pressure
Azoty Tarnow™ TARFLEN SM-B40 PTFE
Reinforced with 40% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Back Pressure 50.0 - 70.0 MPa
7250 - 10200 psi
Molding Pressure
Azoty Tarnow™ TARFLEN SM-S25 PTFE
Tarflen SM1 reinforced with 25% glass fiber for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.