Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 103 MPa | 15000 psi | Mold pressure |
Oxford Polymers 30GF 30% Glass Fiber Filled Polycarbonate for Injection Molding 30% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Back Pressure | 103 MPa | 15000 psi | Mold pressure |
Oxford Polymers 40GF 40% Glass Fiber Filled Polycarbonate for Injection Molding 40% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Back Pressure | 103 MPa | 15000 psi | Mold pressure |
Oxford Polymers 20GF 20% Glass Fiber Filled Polycarbonate for Injection Molding 20% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |