Polymer Property : Back Pressure = 6.89 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 0.000 - 6.89 MPa
0.000 - 1000 psi
Injection
Lubrizol Estane® 58070 Thermoplastic Polyurethane
Features: Outstanding resiliency, fuel resistance and low temperature flexibility.Uses: Hose and Tube, Injection Molding, Fabric Coating and Wire/CableAvailable in Americas, Europe, Middle East, Afr..