Polymer Property : Back Pressure = 80.0 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Molding Pressure
Azoty Tarnow™ TARFLEN SM-B60 PTFE
Tarflen SM1 reinforced with 60% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.