Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 15 - 75 rpm | 15 - 75 rpm | |
PolyOne Versaflex™ CL2000X Thermoplastic Elastomer (TPE) Versaflex™ CL2000X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and an extremely soft feel are desired. - Tactile Feel - Ultra-Soft - Water Clar.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020GX6 Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, glass fiber reinforced, UV resistanceInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020LU1X3 Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020X8 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3024LU Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3024U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethylacetate for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethylene Glycol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Saturate Sodium Chloride for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® P3014UMX Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Screw Speed | 15 - 40 rpm | 15 - 40 rpm | |
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JI6L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for multilayer tubeInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Fuel C/E10 for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Methanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Saturate Sodium Chloride for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sulfuric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sulfuric Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Trichloroethylene for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Water for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Zinc chloride aq. for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3035UF Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Screw Speed | 15 - 70 rpm | 15 - 70 rpm | |
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryerUses: Extrusion: Cable jacket, hose/tube, profile and film and .. |