Processing Properties Metric English Comments
Cure Time 0.830 min
0.0138 hour
Loctite® 408 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Cure Time 0.830 min
0.0138 hour
Loctite® PRISM® 403 Instant Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..