Processing Properties Metric English Comments
Cure Time 6.00 - 7.80 min

@Temperature -55.0 - 200 °C
0.100 - 0.130 hour

@Temperature -67.0 - 392 °F
Handling
Palm Labs Adhesives TURBO-LOCK SERIES 11-HT Anaerobic Thread Locking Compound
TURBO-LOCK 11-HT SERIES is a fast curing, BLUE, removable, medium strength, high temperature, anaerobic thread-locking compound for bonding and sealing threads. It is highly resistance to heat, vibr..