Processing Properties Metric English Comments
Cure Time 10 - 15 min
0.17 - 0.25 hour
Fixture
Loctite® 3035™ Polyolefin Bonder
Loctite® 3035™ Polyolefin Bonder is an easy-to-use, 1:1 mix product that can be stored at room temperature and works where traditional low surface energy bonders often fail. Loctite® 3035™ Polyo..