Polymer Property : Cure Time = 0.192 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 5.50 - 11.5 min
0.0917 - 0.192 hour
t`50; ASTM D2084
ExxonMobil Exxon™ 6222 Brominated Star-Branched Butyl
Exxon SB Bromobutyl is a brominated copolymer of isobutylene and isoprene, including a styrene block copolymer branching agent.Information provided by ExxonMobil Chemical