Cure Time 21.0 min

@Temperature 154 °C
0.350 hour

@Temperature 310 °F
Press cured
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Mistron Vapor Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Cure Time 21.0 - 29.0 min
0.350 - 0.483 hour
t`90; ASTM D2084
ExxonMobil Exxon™ 4266 Star-Branched Butyl
Exxon SB Butyl is a copolymer of isobutylene and isoprene, including a styrene block copolymer branching agent.Information provided by ExxonMobil Chemical
Cure Time 21.0 min
0.350 hour
Tack Free Time, 50% RH
3M Impact Protection Adhesive
3M Impact Protection Adhesive improves the overall performance of 3M Safety and Security Window Films. This unique window protection system combines the toughness of 3M patented micro-layer safety f..
Cure Time 21.0 min

@Temperature 154 °C
0.350 hour

@Temperature 310 °F
Press cured
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Mistron Vapor Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..