Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 22.0 min @Temperature 68.3 °C |
0.367 hour @Temperature 155 °F |
Press cured |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 22.0 min @Temperature 154 °C |
0.367 hour @Temperature 310 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR Laminar Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 22.0 min @Temperature 154 °C |
0.367 hour @Temperature 310 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Benzoflex 9-88SG Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 22.0 min @Temperature 154 °C |
0.367 hour @Temperature 310 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Benzoflex 9-88SG Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 22.0 min @Temperature 68.3 °C |
0.367 hour @Temperature 155 °F |
Press cured |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 22.0 min | 0.367 hour | Tack-Free, 50% RH |
3M 4000 UV 5280 Marine Adhesive/Sealant Fast Cure 3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio.. |
|||
Cure Time | 22.0 min | 0.367 hour | Tack-Free, 50% RH |
3M 4000 UV 6580 Marine Adhesive/Sealant Fast Cure 3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio.. |
|||
Cure Time | 22.0 min | 0.367 hour | Tack-Free, 50% RH |
3M 4000 UV 6586 Marine Adhesive/Sealant Fast Cure 3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio.. |
|||
Cure Time | 22.0 min @Temperature 154 °C |
0.367 hour @Temperature 310 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR Laminar Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |