Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 35.0 min @Temperature 154 °C |
0.583 hour @Temperature 310 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TP-95 Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 35.0 min @Temperature 154 °C |
0.583 hour @Temperature 310 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TP-95 Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |