Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.783 - 0.917 min | 0.0131 - 0.0153 hour | per mm |
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App.. |
|||
Cure Time | 0.783 - 0.917 min | 0.0131 - 0.0153 hour | per mm |
Amity Thermosets ATO 159 Phenolic Molding Glass/ inorganic Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |