Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 1.08 - 1.33 min | 0.0181 - 0.0222 hour | per mm |
Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color.. |