Processing Properties Metric English Comments
Cure Time 11.5 min

@Temperature 68.3 °C
0.192 hour

@Temperature 155 °F
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.25 PHR Zinc Stearate
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Cure Time 11.5 min

@Temperature 68.3 °C
0.192 hour

@Temperature 155 °F
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.25 PHR Zinc Stearate