Cure Time 1260 min
21.0 hour
3M AC-665 Class C-24 Aerospace Sealant
3M Aerospace Sealant AC-665 Class C are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros..