Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 20.0 min | 0.333 hour | On steel (fixture) |
ND Industries StudGrade® 140 Permanent Threadlocker General DescriptionHigh strength threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical Usesstuds and bolts, and threaded pipe fittings.Meets m.. |
|||
Cure Time | 20.0 - 25.0 min | 0.333 - 0.417 hour | working strength |
Permabond TA4202 Toughened Acrylic Adhesive PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
Cure Time | 20.0 min | 0.333 hour | handling time, .5 mm gap |
Permabond TA430 Acrylic Adhesive & Initiator PERMABOND TA430 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics, wood, and some thermoplastics. This adhesive may be used in a variety of structural bondin.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N220 (ISAF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N774 (SRF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 70 PHR N550 (FEF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 70 PHR N774 (SRF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 - 25.0 min | 0.333 - 0.417 hour | Fixture time |
ITW Devcon Metal Welderâ„¢ Methacrylate Adhesive, Grey / Beads Information provided by ITW Devcon |
|||
Cure Time | 20.0 min | 0.333 hour | Tack-free |
Momentive Performance Materials RTV118 One Component Acetoxy Adhesive Sealant, Translucent RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Cure Time | 20.0 min @Pressure 0.207 MPa, Temperature 40.0 °C |
0.333 hour @Pressure 30.0 psi, Temperature 104 °F |
|
Lucite International Colacryl ® D1-120 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I.. |
|||
Cure Time | 20.0 min @Temperature 150 °C |
0.333 hour @Temperature 302 °F |
|
Lord Adhesives Circalokâ„¢ EP-939 Epoxy Board Level Encapsulant LORD Thermosetâ„¢ EP-939 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N774 (SRF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR N330 (HAF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 154 °C |
0.333 hour @Temperature 310 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Control Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | >= 20.0 min | >= 0.333 hour | |
Trelleborg Emerson & Cuming Stycast® 5952 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N550 (FEF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N774 (SRF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N550 (FEF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min | 0.333 hour | |
Loctite® 222MS Low Strength/Small Screw Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Cure Time | 20.0 min | 0.333 hour | Tack-free |
Loctite® 5900 Form-in-place Heavy Body RTV Silicone Heavy Body Flange Sealant Silicone GasketingLoctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing formulations for cure-in-place.. |
|||
Cure Time | 20.0 min | 0.333 hour | Tack-free |
Loctite® 5910 Form-in-place RTV Silicone Flange Sealant Silicone GasketingLoctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing formulations for cure-in-place.. |
|||
Cure Time | 20.0 - 30.0 min | 0.333 - 0.500 hour | |
BCC Products DP-11-75 Urethane Adhesive DP-11-75 is a two component medium viscosity urethane patch system. A hybrid product which was designed specifically for making quick responsive repairs/buildups to the MB 4000 Foundry Plank. DP-11-.. |
|||
Cure Time | 20.0 min | 0.333 hour | Handling Strength |
3M Scotch-Weld™ DP-105 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s.. |
|||
Cure Time | <= 20.0 min | <= 0.333 hour | Fixture Time |
3M Scotch-Weld™ TL72 Threadlocker Anaerobic Adhesive 3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR N774 (SRF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 154 °C |
0.333 hour @Temperature 310 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Control Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N774 (SRF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 154 °C |
0.333 hour @Temperature 310 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Mistron Vapor Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |