Processing Properties Metric English Comments
Cure Time 1200 min

@Temperature 190 °C
20.0 hour

@Temperature 374 °F
Humiseal 1A27 Urethane Conformal Coating
Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit..
Cure Time 1200 min

@Temperature 190 °C
20.0 hour

@Temperature 374 °F
Humiseal 1A27LSE Urethane Conformal Coating
Humiseal 1A27LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingPasses thermal shock test (MIL-I-46058C)..
Cure Time 1200 min

@Temperature 190 °C
20.0 hour

@Temperature 374 °F
Humiseal 1A33 Urethane Conformal Coating
Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL..
Cure Time 1200 min

@Temperature 190 °C
20.0 hour

@Temperature 374 °F
Humiseal 1A33LSE Urethane Conformal Coating
Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther..
Cure Time 1200 min
20.0 hour
Tack-Free Time
3M AC-665 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-665 Class B are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros..