Polymer Property : Cure Time = 21000 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 21000 min

@Time 3600 - 7200 sec
350 hour

@Time 1.00 - 2.00 hour
2nd cure
Aremco Ceramacoat™ 512-N High Temperature Potting & Casting Material Silica
Viscous, off-white paste for circuit breakers, power resistors and solenoids to 240°F (1316°C)