Polymer Property : Cure Time = 23.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 23.0 min

@Temperature 154 °C
0.383 hour

@Temperature 310 °F
Press cured
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Laminar Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Cure Time 23.0 min

@Temperature 154 °C
0.383 hour

@Temperature 310 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Cumar P-10 Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Cure Time 23.0 min

@Temperature 154 °C
0.383 hour

@Temperature 310 °F
Press cured
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Laminar Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Cure Time 23.0 min

@Temperature 154 °C
0.383 hour

@Temperature 310 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Cumar P-10 Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..