Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 200 min | 3 hour | Tack-free |
Momentive Performance Materials RTV5222 Neutral Cure, One Component RTV Adhesive Sealant RTV5220 series sealants are alkoxy neutral cure, one-component, ready to use silicone adhesive sealants exhibiting low modulus/high elongation that will maintain a strong bond even when exposed to e.. |
|||
Cure Time | 200 min | 3 hour | Tack-free |
Momentive Performance Materials RTV5223 Neutral Cure, One Component RTV Adhesive Sealant RTV5220 series sealants are alkoxy neutral cure, one-component, ready to use silicone adhesive sealants exhibiting low modulus/high elongation that will maintain a strong bond even when exposed to e.. |
|||
Cure Time | 200 min | 3 hour | Tack-free |
Momentive Performance Materials RTV5229 Neutral Cure, One Component RTV Adhesive Sealant RTV5220 series sealants are alkoxy neutral cure, one-component, ready to use silicone adhesive sealants exhibiting low modulus/high elongation that will maintain a strong bond even when exposed to e.. |