Cure Time 1800 min

@Temperature 170 °C
30.0 hour

@Temperature 338 °F
Humiseal 1A27 Urethane Conformal Coating
Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit..
Cure Time 1800 min

@Temperature 170 °C
30.0 hour

@Temperature 338 °F
Humiseal 1A27LSE Urethane Conformal Coating
Humiseal 1A27LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingPasses thermal shock test (MIL-I-46058C)..
Cure Time 1800 min

@Temperature 170 °C
30.0 hour

@Temperature 338 °F
Humiseal 1A33 Urethane Conformal Coating
Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL..
Cure Time 1800 min

@Temperature 170 °C
30.0 hour

@Temperature 338 °F
Humiseal 1A33LSE Urethane Conformal Coating
Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther..
Cure Time 1800 min
30.0 hour
Cover mold with polyethylene sheet or locate in a humidity chamber for 24 hrs; 3 hrs at 200°F; 3 hrs at 250°F
Aremco Ceramacast™ 510 High Temperature Potting & Casting Material Alumina
Coarse grain castable for producing large hi-temp tooling.
Cure Time 1800 min
30.0 hour
Tack-Free Time
3M AC-240 Class B-4 Aerospace Sealant
3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan..
Cure Time 1800 min
30.0 hour
3M AC-240 Class B-4 Aerospace Sealant
3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan..