Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 200 min | 4 hour | Tack-free |
Momentive Performance Materials RTV142 White, Low Volatile, One Component Silicone Sealant RTV 142 one-component, ready-to-use adhesive sealant cures to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Methyl alcohol vapors are released.. |
|||
Cure Time | 200 min | 4 hour | Tack-free |
Momentive Performance Materials RTV160 Electronic Grade Silicone Adhesive Sealant, White RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Cure Time | 200 min | 4 hour | Tack-free |
Momentive Performance Materials RTV162 Electronic Grade Silicone Adhesive Sealant, White RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Cure Time | 200 min | 4 hour | Tack-free |
Momentive Performance Materials RTV167 Electronic Grade Silicone Adhesive Sealant, Gray RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |