Polymer Property : Cure Time = 49.8 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 49.8 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.830 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Arlon 51986RA020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the producti..