Processing Properties Metric English Comments
Cure Time 5.10 min
0.0850 hour
Curelastmeter
Daikin DAI-EL G-501NK Fluoroelastomer Terpolymer, Diamine Curable Grade, 68% Fluorine Content
Features: Good mechanical characteristics.Information provided by Daikin Industries.